Procedures tried and tested:
1) Putting scotch tape on the 3 sides of the fused glass before pouring the laminating liquid ( kasi ang tendency nya is tumutulo un liquid nag leleak eh) once poured so properly sealed sya pag merong tape.
2) Meron sya dapat na definite na thickness, so ang product ko kung 3mm thick ang top at bottom glass, ang thickness naman ng glue nya dapat pag natuyo is (3 mm din), so lahat ang thickness nya dapat ay standard na (9 mm).
3) Then i created this "spacer" that i call, ung prang gapper lng sya na habang tine-tape ko ung 3 sides ng glass eh nkapalaman sya sa gitna then pag properly sealed na eh hinuhugot ko na lng ung spacer ko pra ma define ung thickness, but then when i pour the laminating liquid, ang end result is panget pa din eh. especially ung sides nya andaming bako-bako, maski i sanded (niliha) it many times, still same result.
* so un na ang nagiging concern ko, papaano kikinis ung sides nya even kinisin ko ito at papaanong procedures pa kaya ang pwede kong ma-try.
maraming salamat guys